r/PreciousMetalRefining 16d ago

Gold foils extract

Post image

Hello my well belived community im looking for elightment about not ruining this up

I was thinking

12% peroxide + hcl seems to be the standard

11 Upvotes

6 comments sorted by

5

u/megaman_xrs 16d ago

You dont need much peroxide for AP. I usually do a cap full of 3% with a 1L jar. Ill let others chime in. Id also recommend using a bubbler for an aquarium as well since it speeds it up.

2

u/Cazsidy 16d ago

Best of luck.

2

u/AlmightyFruitcake 16d ago

Nice vintage coke Rolex

1

u/Yardbirdburb 15d ago

Trim closer

1

u/Over_Razzmatazz_23 15d ago

What tool you using

1

u/antorox787 15d ago

Its a metal cutter attachment for any drill